French Version

German Version


 

Material: Mallory 3950
     
Nominal Composition: 95% tungsten - nickel - iron
     
     
TYPICAL PROPERTIES    
     
Density: 18.1 gm/cm3
     
Hardness: 30 Rockwell "C"
  (approx. 278 HV)
  (approx. 276 HB30)
     
UTS: 870 MN/m2
     
Electrical Conductivity: 12% microhm cm
     
Specific Resistivity: 83 W/mK  
     
Thermal Conductivity:    
     
Elongation % on 24mm: 16%  
     
Coefficient of Linear Expansion: (20 - 800 deg C) 5.3 x 10-6 in/in/deg.C
     
0.1% Proof Stress: 555 MN/m2

 

All Mallory Alloys Group products conform to, if not exceed, the relevant standards as assured by the Quality Management System Quality Management System - ISO 9002, EN 29002, BS5750-2