French Version

German Version


Material: Mallory 2000
     
Nominal Composition: 95% tungsten - nickel - copper
     
     
TYPICAL PROPERTIES    
     
Density: 18.0 gm/cm3
     
Hardness: 26 Rockwell "C"
  (approx. 255 HV)
  (approx. 255 HB30)
     
UTS: 710 MN/m2
     
Electrical Conductivity: 16% I.A.C.S
     
Specific Resistivity: 10.76 microhm cm
     
Thermal Conductivity: 137.33 W/mK
     
Elongation % on 24mm: 3%  
     
Coefficient of Linear Expansion: (20 - 800 deg C) 5.05 x 10-6 in/in/deg.C

 

All Mallory Alloys Group products conform to, if not exceed, the relevant standards as assured by the Quality Management System Quality Management System - ISO 9002, EN 29002, BS5750-2


© Copyright 2004 Mallory Group Limited, all rights reserved.