Material: Mallory 3925
   
Nominal Composition: 92.5% tungsten – nickel - copper
   
TYPICAL PROPERTIES  
   
Density: 17.5 gm/cm3
   
Hardness: 23 Rockwell “C”
  (approx. 235 HV)
  (approx. 237 HB30)
   
UTS: 718 MN/m2
   
Specific Resistivity: 11 microhm cm
   
Thermal Conductivity: 99 W/mK
   
Elongation % on 24mm: 3%
   
Coefficient of Linear Expansion: (20 – 800 deg C) 5.6 x 10-6 in/in/deg.C

 