DATA SHEET
Material:
Elkanite
20K3
Nominal
Composition:
67% tungsten-carbide 33% copper
Hardness:
105 - 112 Rockwell 'B'
(approx. 278 - 385 HV)
(approx. 276 - 370 HB30)
U.T.S:
685MN/m2
Electrical
Conductivity:
20 - 35% I.A.C.S.
(11.60 - 20.30 M/ohm mm2)
Specific
Resistivity:
8.620 - 4.920 microhm cm
(20
- 900 degs C):
10.1 x 10-6 in/in/deg C
Softening
Temperature:
Approx. 1000 deg C